Buscar
Mostrando ítems 1-2 de 2
Análise da microestrutura, parâmetros térmicos e de propriedades mecânicas na solidificação de ligas com alto teor de cobre Al-(x)%Cu-7%Si
(Universidade Federal de São Carlos, 2019-02-26)
Ternary Al-15%Cu-7%Si and Al-22%Cu-7%Si alloys specimens were obtained by transient directional solidification (DS). This technique is able to provide a very large range of cooling rates and microstructures to be correlated ...
Evolução microestrutural e propriedades mecânicas das ligas Al-10%Si-0,45%Mg e Al-10%Si-1,0%Mg
(Universidade Federal de São Carlos, 2021-07-28)
Al-Si alloys with high silicon (Si) content are widely used in aerospace, automotive, microelectronics, among others. In this context, the Al-10 wt.% Si alloys with the addition of Magnesium (Mg) are alternatives that ...