Search
Now showing items 211-220 of 256
Identificação das variáveis que ocasionam a variação de tonalidade utilizando a técnica de decoração por cilindros de silicone gravados a laser
(Universidade Federal de São Carlos, 2015-11-30)
A major problem in the production of ceramic tiles for coating is the variation of
tonality. The determination of their origin within the entire production process and to
minimize its occurrence by the manufacturer is ...
Avaliação da durabilidade do concreto utilizado em postes em São Luís
(Universidade Federal de São Carlos, 2016-06-20)
Reinforced concrete structures built in coastal areas, such as electricity distribution poles, are constantly attacked by aggressive environmental agents. Rebar corrosion mechanism is a specific manifestation of electrochemical ...
Avaliação de corrosão sob tensão e corrosão-fadiga do aço API 5L X70 em solução etanólica sintética
(Universidade Federal de São Carlos, 2022-04-07)
API X70 steel has been widely used in Brazil for the manufacture of ethanol transport pipelines, however, a recognized problem in carbon steel pipes exposed to ethanol is stress corrosion cracking (SCC) and, in addition, ...
Influência da adição de um fundente sintético no mecanismo de coloração final de revestimentos cerâmicos
(Universidade Federal de São Carlos, 2011-08-12)
The presence of iron oxide in ceramic tile mass contributes to the reddish color firing of the products leading to a lower aggregate value, not to be regarded as a "noble" ceramic. However, the use of raw materials with ...
Sinterização, cristalização, desenvolvimento e caracterização de vitrocerâmicas de baixo coeficiente de expansão térmica do sistema Li2O - Al2O3 SiO2 (LAS)
(Universidade Federal de São Carlos, 2010-10-15)
Glass-ceramics based on the Li2O-Al2O3-SiO2 (LAS) system represent the most important (commercial) family. They are required for applications where extreme dimensional stability and thermal shock resistance are of utmost ...
Cristalização e sinterização de bio vidros do sistema Na2O-CaO-SiO2-P2O5
(Universidade Federal de São Carlos, 2001-03-30)
The objective of this work was to study crystallisation and sintering of Bio-glasses of Na2O CaO SiO2 P2O5 aiming at the improvement of the mechanical properties. In order to study the development of glass-ceramics in this ...
Novas ligas formadoras de fase amorfa do sistema Ni-Nb-Zr e seu comportamento mecânico
(Universidade Federal de São Carlos, 2011-04-15)
Ni-based amorphizable alloys in the bulk form show a good combination of properties, with high mechanical strength and hardness, good ductility and excellent corrosion resistance. These alloys have been used in recent ...
Degradação da resistência à corrosão de aços inoxidáveis duplex, devido ao envelhecimento em baixas temperaturas por tempos prolongados.
(Universidade Federal de São Carlos, 2004-08-30)
Although duplex stainless steels exhibit good performance in many severe corrosive environments, their corrosion resistance can be hampered by precipitation of chromium (Cr) rich phases during aging heat treatments.
Micr ...
Caracterização da resistência à corrosão de ligas inoxidáveis Fe-Mn-Si-Cr-Ni-(Co) com efeito de memória de forma
(Universidade Federal de São Carlos, 2011-03-03)
In this work, the corrosion behavior of three Fe-Mn-Si-Cr-Ni (Co) shape memory stainless steels (SMSS) in aggressive environments was characterized. The electrochemical corrosion behavior in 0.5 M H2SO4 solution was obtained ...
Avaliação do dano por choque térmico em concretos refratários via espectroscopia acústica ressonante não-linear
(Universidade Federal de São Carlos, 2012-03-02)
In this thesis the Non-linear Resonant Acoustic Spectroscopy Technique used to evaluate the mesoscopic non-linearity was incorporated into the Impulse Excitation Technique, which is extensively applied to the evaluation ...